Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 4.8 cSt | 4.8 cSt | |
ConocoPhillips 32 Spectrum Cutting Oil Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica.. |