Polymer Property : Kinematic Viscosity at 100°C (212°F) = 4.7 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 4.7 cSt
4.7 cSt
Base Oil; ASTM D445
Nye Lubricants 716R (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 4.7 cSt
4.7 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8110 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 4.7 cSt
4.7 cSt
ASTM D445
ChevronTexaco 5R Neutral Oil
FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o..
Kinematic Viscosity at 100°C (212°F) 4.7 cSt
4.7 cSt
ASTM D445
ExxonMobil Synesstic™ 5 Synthetic Fluid
Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit..