Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 4.36 cSt | 4.36 cSt | ASTM D445 |
ChevronTexaco ISO 32 Machine Oil R&O LVI FeaturesChevron Machine Oil R&O LVI is a superior quality naphthenic lubricating oilIt is formulated with highly refined base stock with rust inhibiting, antioxidant, and foam suppressant additives... |