Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | Base Oil; ASTM D445 |
Nye Lubricants 811-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | ASTM D445 |
ExxonMobil 603 Mobiltherm 600 Series Mobiltherm heat transfer oils are high performance products intended for use in closed indirect heating installations. They are formulated from highly refined base stocks that are resistant to therm.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | ASTM D445 |
ExxonMobil 763 Mobilmet 760 Series Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | ASTM D445 |
ExxonMobil Mobil Zerice 32 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | ASTM D445 |
ChevronTexaco Elite-Cut® NL Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | ASTM D445 |
ExxonMobil 763 Mobilmet 760 Series Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | ASTM D445 |
ExxonMobil Mobil Zerice 32 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Kinematic Viscosity at 100°C (212°F) | 4.2 cSt | 4.2 cSt | ASTM D445 |
ExxonMobil 603 Mobiltherm 600 Series Mobiltherm heat transfer oils are high performance products intended for use in closed indirect heating installations. They are formulated from highly refined base stocks that are resistant to therm.. |