Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | Base Oil; ASTM D445 |
Nye Lubricants 176 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | Base Oil; ASTM D445 |
Nye Lubricants 176A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | Base Oil; ASTM D445 |
Nye Lubricants 176F (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | Base Oil; ASTM D445 |
Nye Lubricants 176H (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | |
ConocoPhillips Syncon® 320 Synthetic EP Gear Oil, AGMA No. 6EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® 6460 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 460 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |
|||
Kinematic Viscosity at 100°C (212°F) | 38 cSt | 38 cSt | |
ConocoPhillips Inca® 680 Oil, AGMA No. 8 Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |