Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 35.8 cSt | 35.8 cSt | ASTM D445 |
ExxonMobil Extra Hecta Super Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Kinematic Viscosity at 100°C (212°F) | 35.8 cSt | 35.8 cSt | |
ChevronTexaco Pinnacle® EP 320 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Kinematic Viscosity at 100°C (212°F) | 35.8 cSt | 35.8 cSt | ASTM D445 |
ChevronTexaco TEGRA® ISO 320 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Kinematic Viscosity at 100°C (212°F) | 35.8 cSt | 35.8 cSt | ASTM D445 |
ExxonMobil Extra Hecta Super Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |