Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 100°C (212°F) = 31.5 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 31.5 cSt
31.5 cSt
ASTM D445
ExxonMobil 34 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Kinematic Viscosity at 100°C (212°F) 31.5 cSt
31.5 cSt
ASTM D445
ChevronTexaco ParaMount™ ELV Paraffinic Process Oil
FeaturesChevron ParaMount ELV Paraffinic Process Oil offers all the advantages of a bright stock including low weight loss and excellent solubility.ELV is exceptional because of its very light color..
Kinematic Viscosity at 100°C (212°F) 31.5 cSt
31.5 cSt
ASTM D445
ExxonMobil 34 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Kinematic Viscosity at 100°C (212°F) 31.5 cSt
31.5 cSt
Base Oil
ConocoPhillips 1 HD Calcium Grease NLGI No. 1
Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive..
Kinematic Viscosity at 100°C (212°F) 31.5 cSt
31.5 cSt
Base Oil
ConocoPhillips 2 HD Calcium Grease NLGI No. 2
Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive..