Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 3.28 cSt | 3.28 cSt | ASTM D445 |
ExxonMobil Mobil Velocite 8 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |
|||
Kinematic Viscosity at 100°C (212°F) | 3.28 cSt | 3.28 cSt | ASTM D445 |
ExxonMobil Mobil Velocite 8 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |