Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 3.2 cSt @Temperature 100 °C |
3.2 cSt @Temperature 212 °F |
ASTM D445 |
PolyOne Synplast™ DOS-N Di (2-ethylhexyl) Sebacate Branched C8 sebacate esterInformation provided by PolyOne |
|||
Kinematic Viscosity at 100°C (212°F) | 3.2 cSt | 3.2 cSt | ASTM D445 |
ExxonMobil Mobil Zerice 15 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Kinematic Viscosity at 100°C (212°F) | 3.2 cSt | 3.2 cSt | ASTM D445 |
ChevronTexaco ISO 15 Handy Oil FeaturesChevron Handy Oil is a highly refined, light-bodied, multipurpose lubricating oil.It contains an oxidation inhibitor to improve its natural stability and prevent the formation of gums and va.. |
|||
Kinematic Viscosity at 100°C (212°F) | 3.2 cSt | 3.2 cSt | ASTM D445 |
ExxonMobil Exterex™ A34 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Kinematic Viscosity at 100°C (212°F) | 3.2 cSt | 3.2 cSt | ASTM D445 |
ChevronTexaco Vapor Space Rust Inhibitor Concentrate FeaturesChevron Vapor Space Rust Inhibitor Concentrate is formulated to prevent rusting in lubricating oil systems in areas above the oil level for units such as gear cases, oil reservoirs, bearing .. |
|||
Kinematic Viscosity at 100°C (212°F) | 3.2 cSt | 3.2 cSt | ASTM D445 |
ExxonMobil Mobil Zerice 15 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Kinematic Viscosity at 100°C (212°F) | 3.2 cSt | 3.2 cSt | ASTM D445 |
ChevronTexaco Bright-Cut® AD Metal Working Fluid FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components .. |