Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants 300 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368A (NC-GP) (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368AS (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants NC-125 Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants NC-GP Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8180 (479) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8182 (837) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8182R (837RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | ASTM D445 |
ExxonMobil 220 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil |
ConocoPhillips Tacna® HD Grease NLGI Grade 2 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | ASTM D445 |
ExxonMobil 220 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 100°C (212°F) | 26 cSt | 26 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368S (RL) Synthetic Oil Information provided by Nye Lubricants. |