Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 24.4 cSt | 24.4 cSt | ASTM D445 |
ExxonMobil AA Mobil DTE Oil Double Letter Series The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing.. |
|||
Kinematic Viscosity at 100°C (212°F) | 24.4 cSt | 24.4 cSt | ASTM D445 |
ExxonMobil AA Mobil DTE Oil Double Letter Series The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing.. |