Polymer Property : Kinematic Viscosity at 100°C (212°F) = 23.4 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 23.4 cSt
23.4 cSt
ChevronTexaco 320 Honor Ashless AW
Texaco Honor Ashless AW are circulating oils formulated from high quality base stocks and a carefully balanced, zinc-free additive package. These proved excellent protection against wear for long be..
Kinematic Viscosity at 100°C (212°F) 23.4 cSt
23.4 cSt
ASTM D445
ChevronTexaco ISO 320 Machine Oil AW
FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu..
Kinematic Viscosity at 100°C (212°F) 23.4 cSt
23.4 cSt
Base Oil
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1
Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic ..
Kinematic Viscosity at 100°C (212°F) 23.4 cSt
23.4 cSt
Base Oil
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1
Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic ..