Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 22.3 cSt
22.3 cSt
ASTM D445
ChevronTexaco Dura-Lith® NLGI 000 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Kinematic Viscosity at 100°C (212°F) 22.3 cSt
22.3 cSt
Base Oil
ConocoPhillips Grade 1 Calcium M Grease NLGI
Description: Conoco Calcium M Grease is a specialty product that incorporates high load-carrying and antiwear capabilities with excellent low temperature properties and high-temperature stability af..