Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | Base Oil; ASTM D445 |
Nye Lubricants 761G Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | ASTM D445 |
ExxonMobil Mobil Synthetic Oven Lube 1090 Mobil Synthetic Oven Lube 1090 is a supreme performance synthetic high temperature lubricant designed specifically for lubrication of hot conveyor chains in drying ovens and similar severe applicati.. |
|||
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | |
ConocoPhillips Syncon® 150 Synthetic EP Gear Oil, AGMA No. 4EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | ASTM D445, DIN 51 519 |
Chesterton 610 MT Plus Synthetic Lubricating Fluid Description: Chesterton® 610 MT Plus Synthetic Lubricating Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from 25°C (-15°F) to those o.. |
|||
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | ASTM D445 |
ExxonMobil Mobil Synthetic Oven Lube 1090 Mobil Synthetic Oven Lube 1090 is a supreme performance synthetic high temperature lubricant designed specifically for lubrication of hot conveyor chains in drying ovens and similar severe applicati.. |
|||
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 220 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |
|||
Kinematic Viscosity at 100°C (212°F) | 22 cSt | 22 cSt | Base Oil; ASTM D445 |
Nye Lubricants 792D (NG) Synthetic Oil Information provided by Nye Lubricants. |