Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 20.5 cSt | 20.5 cSt | ASTM D445 |
ExxonMobil Enmist EP 320 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 100°C (212°F) | 20.5 cSt | 20.5 cSt | ASTM D445 |
ExxonMobil Enmist EP 320 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |