Polymer Property : Kinematic Viscosity at 100°C (212°F) = 20 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants 231(SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants 272 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants 436 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants 790G (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants 790G-MS (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants NYOSIL-M25 Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants NYOSIL-M25UV Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
ASTM D-445
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150
Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val..
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
ConocoPhillips Hydroclear® 220 TCS Slideway lubricant
Description: Conoco Hydroclear® TCS Slideway Lubricant is a premium demulsible machine tool way lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear TCS Slideway Lubricant ..