Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 2.3 cSt
2.3 cSt
ChevronTexaco Inhibited Transformer Oil
Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer component..
Kinematic Viscosity at 100°C (212°F) 2.3 cSt
2.3 cSt
ChevronTexaco Transformer Oil
Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer component..
Kinematic Viscosity at 100°C (212°F) 2.3 cSt
2.3 cSt
ConocoPhillips Transformer Oil
Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is al..
Kinematic Viscosity at 100°C (212°F) 2.3 cSt
2.3 cSt
Duratherm LT Paraffinic Heat Transfer Fluid
Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminat..
Kinematic Viscosity at 100°C (212°F) 2.3 cSt

@Temperature 100 °C
2.3 cSt

@Temperature 212 °F
ASTM D445
PolyOne Synplast™ DOA-FDA Di (2-ethylhexyl) Adipate
Branched C8 adipate esterInformation provided by PolyOne
Kinematic Viscosity at 100°C (212°F) 2.3 cSt

@Temperature 100 °C
2.3 cSt

@Temperature 212 °F
ASTM D445
PolyOne Synplast™ DOA-N Di (2-ethylhexyl) Adipate
Branched C8 adipate esterInformation provided by PolyOne