Polymer Property : Kinematic Viscosity at 100°C (212°F) = 2.2 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 2.2 cSt
2.2 cSt
ChevronTexaco Concrete Form Oil VOC
Texaco Concrete Form Oil VOC delivers value through:Clean separation from forms — imparts an excellent surface finish to concrete.Minimal build-up on forms — providing longer form lifeRust protect..