Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 2.1 cSt | 2.1 cSt | |
ChevronTexaco Havoline® DOT 3 Brake Fluid Havoline Brake Fluid DOT 3 delivers value through:good brake responselong fluid lifeminimal leakageHavoline Brake Fluid DOT 3 is a nonpetroleum, automotive brake fluid designed for use in convention.. |