Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 171 cSt
171 cSt
Base Oil; ASTM D445
Nye Lubricants 500F (RS) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 171 cSt
171 cSt
ASTM D445
ExxonMobil 3200 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Kinematic Viscosity at 100°C (212°F) 171 cSt
171 cSt
ASTM D445
ExxonMobil 3200 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Copyright © lookpolymers.com All Rights Reserved