Polymer Property : Kinematic Viscosity at 100°C (212°F) = 17 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil; ASTM D445
Nye Lubricants FTL-9000 Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
ASTM D445
ExxonMobil 150 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips SUPER-STA NLGI No. 1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips SUPER-STA NLGI No. 2
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
ConocoPhillips Syncon® 75W-90 HP Synthetic Gear Oil
Description: Conoco Syncon HP Synthetic Gear Oil is recommended for conventional and limited-slip differentials, as well as some manual transmissions commonly found in passenger cars, race cars, tru..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
ELM® 80W90 Multi-Purpose Biodegradable – Biobased Gear Lubricant
Description: ELM 80W90 Multi-Purpose Gear Lubricant is a premium quality biodegradable gear lubricant formulated with the best optimized Biotechbased™ USA-grown natural seed oil that surpasses the ..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
ASTM D445
ExxonMobil 150 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 0
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 00
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 000
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 1
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 2
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips SUPER-STA M NLGI No.0
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips SUPER-STA M NLGI No.2
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
ASTM D445
ChevronTexaco Delo® Synthetic Grease SF
FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature..
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
ConocoPhillips SUPER-STA M NLGI No.1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...