Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 16.5 cSt | 16.5 cSt | ASTM D445 |
ExxonMobil Mobil Almo 529 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Kinematic Viscosity at 100°C (212°F) | 16.5 cSt | 16.5 cSt | ASTM D445 |
ChevronTexaco ISO 220 Marine Oil E FeaturesChevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines... |
|||
Kinematic Viscosity at 100°C (212°F) | 16.5 cSt | 16.5 cSt | ASTM D445 |
ExxonMobil Enmist EP 220 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 100°C (212°F) | 16.5 cSt | 16.5 cSt | ASTM D445 |
ExxonMobil Mobil Almo 529 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Kinematic Viscosity at 100°C (212°F) | 16.5 cSt | 16.5 cSt | ASTM D445 |
ExxonMobil Enmist EP 220 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |