Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 16.1 cSt | 16.1 cSt | ASTM D445 |
ChevronTexaco ECO® SAE 40 Heavy Duty Motor Oil Features:Chevron ECO Heavy Duty Motor Oils are formulated to be environmentally responsible engine lubricants. They use the highest quality re-refined base oils and specially selected additives desi.. |
|||
Kinematic Viscosity at 100°C (212°F) | 16.1 cSt | 16.1 cSt | |
Duratherm S Silicone Heat Transfer Fluid Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s.. |