Kinematic Viscosity at 100°C (212°F) 152 cSt
152 cSt
ASTM D445
ChevronTexaco NC Open Gear Grease
FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases ..
Kinematic Viscosity at 100°C (212°F) 152 cSt
152 cSt
ASTM D445
ChevronTexaco Open Gear Grease
FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases ..
Kinematic Viscosity at 100°C (212°F) 152 cSt
152 cSt
ASTM D445
ChevronTexaco Aerosol Open Gear Grease
FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases ..