Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8510 (487) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ExxonMobil 15W-40 Exxon XD-3 Elite Exxon XD-3 15W-40 is a synthetic blend heavy duty diesel engine oil that provides the highest level of protection to modern, high performance diesel engines used in severe on and off highway applic.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ExxonMobil Mobil Delvac 15W-40 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ChevronTexaco Delo® 400 Multigrade, SAE 15W-40 Features:Chevron Delo 400 Multigrade heavy duty motor oil is a super premium quality "universal" engine oil which exceeds industry and engine manufacturers performance requirements. It is formulated.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ChevronTexaco Delo® 400 Synthetic, SAE 5W-40 Chevron Delo 400 Synthetic heavy duty motor oils are multipurpose 100% synthetic lubricants formulated for use in gasoline and diesel engines, torque converters, gear cases, and hydraulic systems op.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ChevronTexaco HDAX® SAE 15W-40 FeaturesChevron HDAX Ashless Gas Engine Oils are superior quality, ashless, gas engine oils.They are formulated with ISOSYN™ base stocks and a carefully balanced ashless package of dispersant, anti.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ChevronTexaco HDAX® SAE 15W-40 Low Ash Gas Engine Oil FeaturesChevron HDAX Low Ash Gas Engine Oils are high quality, bright stock-free, low ash, dispersant/detergent type engine oils.They are formulated with ISOSYN™ base stocks and an additive package.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | See Note 3. |
ChevronTexaco Multifak® EP NLGI Grade 0 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | See Note 3. |
ChevronTexaco Multifak® EP NLGI Grade 1 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | See Note 3. |
ChevronTexaco Multifak® EP NLGI Grade 2 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ChevronTexaco RPM® SAE 15W-40 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ExxonMobil 15W-40 Exxon XD-3 Elite Exxon XD-3 15W-40 is a synthetic blend heavy duty diesel engine oil that provides the highest level of protection to modern, high performance diesel engines used in severe on and off highway applic.. |
|||
Kinematic Viscosity at 100°C (212°F) | 15.6 cSt | 15.6 cSt | ASTM D445 |
ExxonMobil Mobil Delvac 15W-40 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |