Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 10 - 15 cSt
10 - 15 cSt
ASTM D445, DIN 51 561
Chesterton 610 Synthetic Lubricating Fluid
Description: Chesterton® 610 Synthetic Lubrication Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from -25°C (-15°F) for those over 27..