Polymer Property : Kinematic Viscosity at 100°C (212°F) = 14.4 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
Base Oil; ASTM D445
Nye Lubricants 402 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ExxonMobil Extra Heavy Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
Base Oil
ConocoPhillips Tacna® Rx NLGI No. 1
Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ChevronTexaco Aries® 150
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ChevronTexaco Delo® 1000 Marine Engine Oil, SAE 40
FeaturesChevron Marine Engine Oils Delo 1000 Marine are highquality engine oils developed for use in a wide variety of medium speed trunk piston engines, including the latest design high output engi..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ChevronTexaco Delo® 2000 Marine Engine Oil, SAE 40
FeaturesChevron Marine Engine Oil Delo 2000 Marine is a high quality engine oil developed for use in a wide variety of medium speed trunk piston engines burning marine diesel oils, or residual fuels..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ChevronTexaco Gear Compounds EP, ISO 150
FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure protection, antiwear and demulsibility, oxidation, rust, corrosion control an..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ChevronTexaco Geotex® LA SAE 15W-40
Texaco Geotex LA oils deliver value through:Low maintenance cost and long engine lifeLow wear — Provide excellent protection againstpiston, ring, and liner scuffing, scoring, and wear.Reduced valve..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ChevronTexaco Meropa® 150
Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ExxonMobil Extra Heavy Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D-445
ConocoPhillips ANDEROL® AA-40 White Mineral Food Grade Oil, ISO Grade 150, SAE Grade 40
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 40
Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 15W-40
Conoco® El Mar Ashless Supreme is a premium quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and turbocharged 2-stroke cycle natural gas engines. Engine..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ConocoPhillips El Mar® 3000 Oil SAE Grade 15W-40
Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ConocoPhillips Hydroclear® 150 4 EP gear Oil
Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
Base Oil
ConocoPhillips Moly Poly Grease NLGI No. 2
Description: Conoco Moly Poly Grease is a long-life, lithium 12-hydroxy grease for chassis, wheel bearings, ball joints, U-joints, tie-rod ends, steering knuckles and brake self-adjusting screws fou..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ChevronTexaco Clarity® ISO 100 Synthetic Paper Machine Oil
FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) ..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ChevronTexaco Delo® 3000 Marine Engine Oil, SAE 40
FeaturesChevron Marine Engine Oil Delo 3000 Marine is a high quality engine oils developed for use in a wide variety of medium speed trunk piston engines burning residual fuels.It is manufactured us..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
ChevronTexaco Vistac® ISO 150 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ConocoPhillips Conoco® El Mar® Grade 40 Mid Ash Supreme Oil
Conoco® El Mar Mid Ash Supreme is a premium quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura..
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
Base Oil
ConocoPhillips Tacna® Rx NLGI No. 2
Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor..