Kinematic Viscosity at 100°C (212°F) 13.3 cSt
13.3 cSt
ASTM D445
ExxonMobil Enmist EP 150
Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist ..
Kinematic Viscosity at 100°C (212°F) 13.3 cSt
13.3 cSt
ASTM D445
ChevronTexaco Dura-Lith® NLGI 1 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Kinematic Viscosity at 100°C (212°F) 13.3 cSt
13.3 cSt
ASTM D445
ChevronTexaco Dura-Lith® NLGI 2 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Kinematic Viscosity at 100°C (212°F) 13.3 cSt
13.3 cSt
ASTM D445
ChevronTexaco Dura-Lith® NLGI 3 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Kinematic Viscosity at 100°C (212°F) 13.3 cSt
13.3 cSt
ASTM D445
ExxonMobil Enmist EP 150
Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist ..