Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 12.7 cSt | 12.7 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8160 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 12.7 cSt | 12.7 cSt | |
ChevronTexaco Alcaid® 220 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |