Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 115 cSt | 115 cSt | Base Oil; ASTM D445 |
Nye Lubricants 779 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 115 cSt | 115 cSt | Base Oil; ASTM D445 |
Nye Lubricants 779ZC (NG) Synthetic Oil Information provided by Nye Lubricants. |