Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 113 cSt | 113 cSt | Base Oil; ASTM D445 |
Nye Lubricants 675 Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 113 cSt | 113 cSt | Base Oil; ASTM D445 |
Nye Lubricants 675(IF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 113 cSt | 113 cSt | Base Oil; ASTM D445 |
Nye Lubricants 675A Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 113 cSt | 113 cSt | Base Oil; ASTM D445 |
Nye Lubricants 675A(IF) Synthetic Oil Information provided by Nye Lubricants. |