Polymer Property : Kinematic Viscosity at 100°C (212°F) = 11.2 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ASTM D445
ExxonMobil 27 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ASTM D445
ExxonMobil 27 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ASTM D445
ExxonMobil 30 Mobiltrans HD
Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4.  This product line ..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ConocoPhillips 100 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ConocoPhillips 100 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ConocoPhillips HD Fleet Supreme™ 10W-30 Engine Oil
Description: Conoco HD Fleet Supreme Engine Oil is a high-quality engine oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. It easily satisfies the warr..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ConocoPhillips Hydroclear® 100 Gas Compressor Fluid
Description: Conoco Hydroclear Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality hydrocracked base oil, combi..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ConocoPhillips Hydroclear® 100 Multipurpose R&O Oil, AGMA Lubricant No. 3
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear ..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ConocoPhillips Hydroclear® 3 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 3
Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks..
Kinematic Viscosity at 100°C (212°F) 11.2 cSt
11.2 cSt
ASTM D445
ExxonMobil 30 Mobiltrans HD
Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4.  This product line ..