Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 10.12 cSt | 10.12 cSt | ASTM D445 |
ExxonMobil Mobil Rarus 827 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Kinematic Viscosity at 100°C (212°F) | 10.12 cSt | 10.12 cSt | ASTM D445 |
ExxonMobil Mobil Rarus 827 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |