Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 94.5 cSt | 94.5 cSt | ASTM D445 |
ChevronTexaco Delo® 400 Synthetic, SAE 5W-40 Chevron Delo 400 Synthetic heavy duty motor oils are multipurpose 100% synthetic lubricants formulated for use in gasoline and diesel engines, torque converters, gear cases, and hydraulic systems op.. |