Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 93 cSt | 93 cSt | |
ConocoPhillips Syncon® 100 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Kinematic Viscosity at 40°C (104°F) | 93 cSt | 93 cSt | |
ChevronTexaco Taro® 16 XD SAE 30 Texaco Taro 16 XD delivers value through:Wear protection — Superior antiwear characteristics result in reduced wear on all moving engine components. Controls ring and liner wear through its ability.. |
|||
Kinematic Viscosity at 40°C (104°F) | 93 cSt | 93 cSt | |
ChevronTexaco Texmar 16 SG SAE 30 Texaco Texmar 16 SG delivers value through:Wear protection — Texaco Texmar 16 SG oil has superior anti-wear characteristics to reduce wear on all moving engine components. Controls ring and liner w.. |