Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 9.2 cSt | 9.2 cSt | ASTM D445 |
ExxonMobil Mobilgrease 27 Mobilgrease 27 is a high performance, aviation grease designed to combine the unique features of a synthetic ester base fluid with a lithium soap thickener. Its consistency is between an NLGI No. 1 .. |
|||
Kinematic Viscosity at 40°C (104°F) | 9.2 cSt | 9.2 cSt | ASTM D445 |
ExxonMobil Mobilgrease 27 Mobilgrease 27 is a high performance, aviation grease designed to combine the unique features of a synthetic ester base fluid with a lithium soap thickener. Its consistency is between an NLGI No. 1 .. |