Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 8375 cSt | 8375 cSt | ASTM D445 |
ChevronTexaco 800 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |