Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 830 cSt | 830 cSt | Base Oil; ASTM D445 |
Nye Lubricants 925 (HSC) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 830 cSt | 830 cSt | Base Oil; ASTM D445 |