Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 8.7 cSt | 8.7 cSt | |
ChevronTexaco Inhibited Transformer Oil Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer component.. |