Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 77.8 cSt | 77.8 cSt | |
ConocoPhillips Synterra™ 2 Hydraulic Oil, AGMA No. 2 Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids .. |