Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 77 cSt | 77 cSt | ASTM D445 |
ExxonMobil Teresstic 77 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Kinematic Viscosity at 40°C (104°F) | 77 cSt | 77 cSt | ASTM D445 |
ExxonMobil Teresstic 77 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Kinematic Viscosity at 40°C (104°F) | 77 cSt | 77 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® PQ AA 80 White Mineral Food Grade Gear Oil, ISO Grade 68/100, SAE Gear Oil Grade 80 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |