Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 74 cSt | 74 cSt | ASTM D445 |
ExxonMobil 10W-30 Exxon XD-3 Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. Thes.. |
|||
Kinematic Viscosity at 40°C (104°F) | 74 cSt | 74 cSt | ASTM D445 |
ExxonMobil 10W-30 Exxon XD-3 Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. Thes.. |
|||
Kinematic Viscosity at 40°C (104°F) | 74 cSt | 74 cSt | ASTM D445 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Kinematic Viscosity at 40°C (104°F) | 74 cSt | 74 cSt | ASTM D445 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |