Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 7.6 cSt @Temperature 40.0 °C |
7.6 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DOA-FDA Di (2-ethylhexyl) Adipate Branched C8 adipate esterInformation provided by PolyOne |
|||
Kinematic Viscosity at 40°C (104°F) | 7.6 cSt @Temperature 40.0 °C |
7.6 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DOA-N Di (2-ethylhexyl) Adipate Branched C8 adipate esterInformation provided by PolyOne |