Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 40°C (104°F) = 69 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 69 cSt
69 cSt
ASTM D445
ExxonMobil 68 Mobil EAL Envirosyn H Series
Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper..
Kinematic Viscosity at 40°C (104°F) 69 cSt
69 cSt
ASTM D445
ChevronTexaco Delo® 100 Motor Oil, SAE 20
Chevron Delo 100 Motor Oils are high performance crankcase oils for diesel engines.They are manufactured using selected premium paraffinic base oils and detergent, dispersant, wear control, antioxid..
Kinematic Viscosity at 40°C (104°F) 69 cSt
69 cSt
ELM® SoyFluid™ Hydraulic Industrial (ISO 68) Premium Biodegradable – Biobased Hydraulic Oil
Description: ELM Biotechbased SoyFluid™ Hydraulic Industrial (ISO 46 & 68) are biodegradable hydraulic oils formulated with the best optimized USA grown natural seed oils that surpass the lubricity..
Kinematic Viscosity at 40°C (104°F) 69 cSt
69 cSt
ConocoPhillips Hydroclear® 10W-30 Super All Season and Super Motor Oil
Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, ..
Kinematic Viscosity at 40°C (104°F) 69 cSt
69 cSt
ChevronTexaco URSA® SAE 20 Extra Duty
Texaco Ursa Extra Duty oils deliver value through:Excellent high temperature deposit control. Protects against high temperature oxidation and oil thickening.Special extreme pressure antiwear propert..
Kinematic Viscosity at 40°C (104°F) 69 cSt
69 cSt
ASTM D445
ExxonMobil 68 Mobil EAL Envirosyn H Series
Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper..
Copyright © lookpolymers.com All Rights Reserved