Kinematic Viscosity at 40°C (104°F) 66.6 cSt
66.6 cSt
ASTM D445
ExxonMobil Mobil Rarus 1026 SHC 1000 Series
The Mobil Rarus SHC 1000 Series is a line of supreme performance oils primarily intended for the lubrication of severe duty rotary screw and vane air compressors. They are particularly suited for se..
Kinematic Viscosity at 40°C (104°F) 66.6 cSt
66.6 cSt
ASTM D445
ChevronTexaco HD Soluble Oil
FeaturesChevron Soluble Oils are used broadly in machine shops as multifunctional cutting fluids. They are primarily designed to cool and lubricate the contact point of the tool and the work piece.C..
Kinematic Viscosity at 40°C (104°F) 66.6 cSt
66.6 cSt
ASTM D445
ExxonMobil Mobil Rarus 1026 SHC 1000 Series
The Mobil Rarus SHC 1000 Series is a line of supreme performance oils primarily intended for the lubrication of severe duty rotary screw and vane air compressors. They are particularly suited for se..