Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 66.3 cSt | 66.3 cSt | ASTM D445 |
ChevronTexaco Supreme SAE 10W-30 Synthetic Motor Oil FeaturesChevron Supreme 100% Synthetic Motor Oils are designed for those drivers who demand the ultimate in engine protection. They provide an extra measure of protection for the investment in a spo.. |