Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 6532 cSt | 6532 cSt | ASTM D445 |
ChevronTexaco NC Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Kinematic Viscosity at 40°C (104°F) | 6532 cSt | 6532 cSt | ASTM D445 |
ChevronTexaco Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Kinematic Viscosity at 40°C (104°F) | 6532 cSt | 6532 cSt | ASTM D445 |
ChevronTexaco Aerosol Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |