Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 65.1 cSt | 65.1 cSt | ASTM D445 |
ExxonMobil Heavy Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Kinematic Viscosity at 40°C (104°F) | 65.1 cSt | 65.1 cSt | ASTM D445 |
ExxonMobil Heavy Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |