Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 530 cSt | 530 cSt | Base Oil; ASTM D445 |
Nye Lubricants 310B (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 530 cSt | 530 cSt | Base Oil; ASTM D445 |
Nye Lubricants 310B-RP (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 530 cSt | 530 cSt | Base Oil; ASTM D445 |
Nye Lubricants 760K (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 530 cSt | 530 cSt | Base Oil; ASTM D445 |
Nye Lubricants 760MS-CP (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 530 cSt | 530 cSt | Base Oil; ASTM D445 |
Nye Lubricants 760K-MS (NG) Synthetic Oil Information provided by Nye Lubricants. |