Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 5000 cSt | 5000 cSt | with diluent; ASTM D445 |
ExxonMobil 375 NC Mobiltac Mobiltac 375 NC, 325 NC and 275 NC extra high performance non-leaded, diluent-type, heavy-bodied open gear lubricants designed for a wide variety of open gear and mining applications. They contain a.. |
|||
Kinematic Viscosity at 40°C (104°F) | 5000 cSt | 5000 cSt | with diluent; ASTM D445 |